首页|期刊导航|含能材料|BuNENA和PBT及其复合体系的热安全性研究

BuNENA和PBT及其复合体系的热安全性研究

李文龙 程志鹏 吕佳璐 张宇 王鑫源 吴星亮 冯蒙蒙 雷超刚 徐森

含能材料2026,Vol.34Issue(9):1017-1025,9.
✕
含能材料2026,Vol.34Issue(9):1017-1025,9.DOI:10.11943/CJEM2026121

BuNENA和PBT及其复合体系的热安全性研究

Thermal Safety of BuNENA,PBT,and the BuNENA/PBT Composite System

李文龙 1程志鹏 2吕佳璐 2张宇 2王鑫源 2吴星亮 3冯蒙蒙 4雷超刚 4徐森3

作者信息

  • 1. 南京理工大学化学与化工学院,江苏 南京 210094||航天化学能源全国重点实验室,内蒙合成化工研究所,内蒙古 呼和浩特 010010
  • 2. 南京理工大学化学与化工学院,江苏 南京 210094
  • 3. 南京理工大学化学与化工学院,江苏 南京 210094||国家民用爆破器材质量监督检验中心,江苏 南京 210094
  • 4. 航天化学能源全国重点实验室,内蒙合成化工研究所,内蒙古 呼和浩特 010010
  • 折叠

摘要

Abstract

To comprehensively evaluate the thermal safety of energetic plasticizer/binder composite systems,a multiscale ther-mal analysis strategy was applied to N-butyl-N-(2-nitroxyethyl)nitramine(BuNENA),poly(3,3-bis(azidomethyl)oxetane-co-tetrahydrofuran)(PBT),and a BuNENA/PBT composite system with a mass ratio of 1∶1.Differential scanning calo-rimetry(DSC),non-isothermal kinetic analysis,slow cook-off tests,5 s explosion point tests,and self-accelerating decomposi-tion temperature(TSADT)calculations based on the Semenov model were used to investigate their thermal decomposition behav-ior and thermal safety characteristics.The DSC results showed that BuNENA mainly underwent exothermic decomposition at 180-240℃,whereas PBT decomposed in a higher temperature range of 220-300℃.The BuNENA/PBT composite exhibited two exothermic peaks,and the first exothermic peak shifted to a higher temperature with a reduced low-temperature exothermic intensity,indicating that PBT could suppress the concentrated heat release of BuNENA at relatively low temperatures.Kinetic analysis further showed that the apparent activation energy of the first decomposition stage of BuNENA/PBT increased compared with that of pure BuNENA,suggesting an enhanced thermal decomposition barrier.In the slow cook-off test,the initial reaction temperature increased from 151.6℃for BuNENA to 162.5℃for BuNENA/PBT.The 5 s explosion point increased from 261.5℃to 290.2℃.For a 25 kg package,the no-return temperature(TNR)and SADT of BuNENA/PBT were 134.7℃and 128.1℃,re-spectively,which were higher than those of BuNENA.These results indicate that compounding BuNENA with PBT can reduce low-temperature concentrated exothermicity and improve the thermal safety margin of BuNENA-based energetic composite sys-tems under slow heating,transient thermal stimulation,and storage-related thermal conditions.

关键词

N-丁基硝氧乙基硝胺(BuNENA)/3,3-二叠氮甲基氧丁环与四氢呋喃共聚物(PBT)/含能增塑剂/热分解/热安全性

Key words

BuNENA/PBT/energetic plasticizer/thermal decomposition/thermal safety

分类

军事科技

引用本文复制引用

李文龙,程志鹏,吕佳璐,张宇,王鑫源,吴星亮,冯蒙蒙,雷超刚,徐森..BuNENA和PBT及其复合体系的热安全性研究[J].含能材料,2026,34(9):1017-1025,9.

基金项目

航天化学能源全国重点实验室基金(NKLACP420251B33) (NKLACP420251B33)

含能材料

1006-9941

访问量0
|
下载量0
段落导航相关论文