沈阳工业大学学报2026,Vol.48Issue(5):73-80,8.DOI:10.7688/j.issn.1000-1646.2026.05.10
附加纯镍过渡层CMT焊接铝/钛异种金属
Cold metal transfer welding of aluminum/titanium dissimilar metals with additional pure nickel transition layer
摘要
Abstract
[Objective]Welded joints of aluminum/titanium dissimilar metals can combine the advantages of aluminum alloys and titanium alloys,having low density,high specific strength,corrosion resistance,and other characteristics,and exhibiting excellent electrical conductivity and heat transfer capabilities.Thus,they have been widely used in aerospace,automotive,electronics,ships,and other fields.The technical difficulties in the manufacture of aluminum/titanium dissimilar material components lie in the significant differences in physical and chemical properties and metallurgical incompatibility between aluminum alloys and titanium alloys.Direct welding will produce a large number of brittle and hard intermetallic compounds such as TiAl3,TiAl2,and TiAl in the weld,resulting in welding hot cracking during the solidification process of the molten pool.To improve the performance of the welded joints of aluminum/titanium dissimilar metals,a pure nickel transition layer was adopted to the weld,which regulated the metallurgical reaction in the weld and reduced the welding heat input on the low-melting-point base material side.[Methods]The base materials were 4 mm thick 5052 aluminum alloy and Ti6Al4V titanium alloy.A 0.1 mm thick pure nickel strip,as a transition layer,was applied to the welding end surface of the aluminum alloy,and Ti6Al4V welding wire with a diameter of 1.2 mm was used as the filling material.The cold metal transfer(CMT)welding method was adopted.After multiple rounds of parameter optimization,the optimal welding parameters were determined to be the wire feed rate of 6 m/min and the welding speed of 15 cm/min.Comparative tests were carried out with and without a pure nickel transition layer,and the microstructure and mechanical properties of the joints were analyzed after welding.[Results]The results show that complete and effective joints cannot be obtained after welding without the use of the transition layer,and there are welding defects such as non-fusion and non-penetration in the weld.Dendrites formed from the high-melting-point base material extend into the low-melting-point base material in the solidification process,which results in the formation of penetrating cracks.Complete and good welded joints are obtained after welding of aluminum/titanium dissimilar metals with the use of the pure nickel transition layer.No welding defects are found in macroscopic testing and microscopic analysis,and the transition layer is completely melted during the welding process.After welding,the transition layer forms an element mixing zone of about 300 μm in situ.By using X-ray diffraction(XRD),scanning electron microscopy(SEM),transmission electron microscopy(TEM),and other modern analysis and detection methods,it is determined that a ternary reaction occurs in the region,producing AlNi2Ti,NiTi2,Al3Ni2,and Al3Ni as the main phase products.The joints are all broken in the weld zone during the tensile process,with an average tensile strength of 62 MPa.[Conclusions]Aluminum/titanium dissimilar metals were welded using the CMT welding technology.The welding end surface of the aluminum alloy base material was coated with a 0.1 mm thick pure nickel strip as a transition layer.No welding defects exist in the welded joint.The transition layer completely melts during the welding process and participates in the metallurgical reaction in the weld,forming an approximately 300 μm thick element mixing zone in situ,where the major metallurgical reactions occur and the primary phases are formed.The addition of the transition layer can effectively reduce the heat input on the low-melting-point base material side,and avoid the generation of a large number of Ti-Al brittle intermetallic compounds in the weld,which can result in welding defects.Compared with the welded joint without the addition of the pure nickel transition layer,the use of the transition layer improves the fluidity of the molten pool,and achieves welding penetration on the back of the welded plate.关键词
铝/钛焊接/焊接过渡层/异种金属焊接/CMT焊接/镍过渡层/熔池反应/断口形貌/金属间化合物Key words
aluminum/titanium welding/welding transition layer/dissimilar metal welding/CMT welding/nickel transition layer/molten pool reaction/fracture morphology/intermetallic compound分类
矿业与冶金引用本文复制引用
刘政军,宋春辉,刘治宇..附加纯镍过渡层CMT焊接铝/钛异种金属[J].沈阳工业大学学报,2026,48(5):73-80,8.基金项目
辽宁省自然科学基金项目(2024-BS-096). (2024-BS-096)