| 注册
首页|期刊导航|表面技术|合金化镀锌板表面白亮带缺陷的微观表征

合金化镀锌板表面白亮带缺陷的微观表征

崔桂彬 鞠新华 孟杨 严春莲 马长文

表面技术2026,Vol.55Issue(20):92-101,10.
✕
表面技术2026,Vol.55Issue(20):92-101,10.DOI:10.16490/j.cnki.issn.1001-3660.2026.20.008

合金化镀锌板表面白亮带缺陷的微观表征

Microstructure Characterization of White Band Defects on the Surface of Galvannealed Steel Sheets

崔桂彬 1鞠新华 2孟杨 1严春莲 1马长文1

作者信息

  • 1. 首钢集团有限公司技术研究院,北京 100043||先进钢铁材料智能研发及制造北京市重点实验室,北京 100043
  • 2. 首钢集团有限公司技术研究院,北京 100043||先进钢铁材料智能研发及制造北京市重点实验室,北京 100043||绿色能源产业链关键新材料国家质量标准实验室,河北 唐山 064400
  • 折叠

摘要

Abstract

The work aims to reveal the formation mechanism of white band defects on the surface of galvannealed(GA)steel.Macroscopically,these defects manifest as discontinuous bright white band parallel to the rolling direction,which not only severely impairs the product's appearance but may also adversely affects its subsequent application performance.The experimental material is GA steel,with a base plate of bake-hardening steel,a thickness of 1 mm,and a chemical composition(wt.%)including:C 0.001 5-0.002 5,Si<0.12,Mn 0.5-0.7,Cr 0.02-0.04,and Ti 0.02-0.06.The steel was annealed at 800℃,galvanized in a zinc bath containing 0.1%-0.15%Al,and then alloyed at 490-550℃.Microstructural and compositional analyses were conducted via a focused ion beam field-emission scanning electron microscope combined with an energy-dispersive spectrometer,quantitative compositional analysis of the micro-regions was carried out by electron probe microana-lysis,phase identification was performed through electron backscatter diffraction,and the coating cross-section was precisely sectioned via focused ion beam,followed by characterization of the nanoscale interfacial structure through transmission electron microscopy and energy-dispersive spectrometer mapping.The phase composition,elemental distribution,and interfacial oxide layer characteristics of the defect area and the normal area were compared and analyzed. The experimental results showed that in the white band defect region,the average Fe content was only 7.20wt.%,significantly lower than the 11.32wt.%Fe content in the normal region.The Fe content decreased by approximately 36wt.%,directly indicating that the alloying degree in this region was markedly insufficient.Phase analysis revealed that the defect region retained pure η-Zn phase(Zn),as well as Γ phase(Fe3Zn10),δ1p phase(Fe13Zn126),and a small amount of ζ phase(FeZn13).In contrast,the normal region consisted of Γ phase,δ1p phase,and a very small amount of ζ phase,with no residual pure Zn phase.Further TEM analysis revealed that at the interface of the defect region,there existed an Fe2Al5 inhibition layer with a thickness of less than 20 nm,while at approximately 150 nm from the interface,a continuous and dense Si-Mn oxide layer composed of"rice-grain-shaped"oxide particles closely arranged in a point-chain pattern was found,with its main components being O,Si,and Mn.At the interface of the normal region,no Fe2Al5 inhibition layer was observed,and the Si-Mn oxide layer was sparse and discontinuous,with a small number of round Si-Mn oxide particles distributed.The significant differences in interfacial structure provided crucial evidence for understanding the formation of the defects. During the annealing process,Si and Mn in the substrate underwent selective oxidation,forming a continuous and dense Si-Mn oxide layer and a thinner Fe2Al5 inhibition layer in the defect region.Subsequently,during the alloying process,this oxide layer acted as a physical barrier,hindering the diffusion of Fe atoms into the coating,while the Fe2Al5 inhibition layer failed to decompose in time.Consequently,the Fe-Zn alloying reaction was retarded,resulting in a large amount of residual pure Zn phase and a thinner coating.During skin passing,the defect region with a thinner coating,due to insufficient compression,exhibited a smooth and low-lying pure Zn surface that produced specular reflection,appearing bright white.In the normal region,because the Si-Mn oxide layer was discontinuous,the diffusion of Fe atoms into the coating was almost unaffected,and the Fe2Al5 inhibition layer decomposed rapidly,thus forming a fully alloyed,thicker coating with no residual pure Zn phase.Therefore,the regional difference in the continuity and compactness of the Si-Mn oxide layer on the substrate surface may be the fundamental cause of the bright white band defects.

关键词

合金化镀锌板/白亮带缺陷/EBSD/FIB/TEM

Key words

galvannealed steel sheet/white band defects/EBSD/FIB/TEM

分类

矿业与冶金

引用本文复制引用

崔桂彬,鞠新华,孟杨,严春莲,马长文..合金化镀锌板表面白亮带缺陷的微观表征[J].表面技术,2026,55(20):92-101,10.

表面技术

1001-3660

访问量0
|
下载量0
段落导航相关论文