电焊机2026,Vol.56Issue(10):131-137,7.DOI:10.7512/j.issn.1001-2303.2026.10.17
Q345R钢压力管道全位置自动焊缺陷分析与改进
All-position Automatic Welding Defect Analysis and Solution of Q345R Steel Pressure Pipeline
冯消冰 1孟继慧 2黄小应 2陈强 1程剑林 2傅含富2
作者信息
- 1. 北京博清科技有限公司,北京 100176
- 2. 浙江宁海抽水蓄能有限公司,浙江 宁波 315000
- 折叠
摘要
Abstract
In the process of automatic welding of Q345R steel large diameter pressure pipeline,there are many strip segrega-tion and non-fusion defects in the root of x-groove,the causes of welded defects in pressure pipeline were analyzed by means of TOFD+UT,element content test and microstructure characterization.The results showed that without preheating,severe carbon segregation occurred at the groove root,with local carbon content reaching up to 4.76%(average 2.31%),far exceeding the limit specified by GB/T 713-2014.The high-carbon band exhibited alternating ferrite and lamellar pearlite microstructure with an increased hardening tendency,which was identified as the primary cause of lack-of-fusion defect ini-tiation.Through comprehensive process improvements including preheating(80~140℃),interpass temperature control(≥80℃),8-zone weld bead arrangement,and welding torch angle optimization,the banded structure was basically eliminated.The TOFD+UT inspection qualification rate of weld seam No.2 reached 96%,with robot welding defect length accounting for only 3.3%of the total weld length.关键词
Q345R钢/全位置/自动焊/缺陷分析Key words
Q345R steel/all-position/automatic welding/defect analysis分类
矿业与冶金引用本文复制引用
冯消冰,孟继慧,黄小应,陈强,程剑林,傅含富..Q345R钢压力管道全位置自动焊缺陷分析与改进[J].电焊机,2026,56(10):131-137,7.