| 注册
首页|期刊导航|建筑结构学报|预制钢筋超高性能混凝土模壳混凝土梁柱节点受剪性能研究

预制钢筋超高性能混凝土模壳混凝土梁柱节点受剪性能研究

王朋 尤学辉 史庆轩 王秋维 戎翀

建筑结构学报2026,Vol.47Issue(9):14-28,15.
✕
建筑结构学报2026,Vol.47Issue(9):14-28,15.DOI:10.14006/j.jzjgxb.2026.0135

预制钢筋超高性能混凝土模壳混凝土梁柱节点受剪性能研究

Shear performance of concrete beam-column joints with precast reinforced ultra-high performance concrete shells

王朋 1尤学辉 2史庆轩 1王秋维 1戎翀1

作者信息

  • 1. 西安建筑科技大学土木工程学院,陕西西安 710055||西安建筑科技大学结构工程与抗震教育部重点实验室,陕西西安 710055
  • 2. 西安建筑科技大学土木工程学院,陕西西安 710055
  • 折叠

摘要

Abstract

To investigate the failure mechanisms and mechanical behavior of reinforced concrete beam-column joints with precast ultra-high performance concrete(UHPC)shells,quasi-static tests were conducted on six exterior joints to evaluate their shear behavior.The experimental parameters included the thickness of the precast column UHPC shell,the axial compression ratio of column,and the joint core stirrup ratio.The failure modes and crack propagation of the joints were examined in detail,and the influences of these parameters on the hysteretic curves,load-bearing capacity,and energy dissipation capacity were analyzed.The results indicate that the final failure is primarily characterized by shear failure in the joint core,accompanied by varying degrees of debonding at the beam-column interface and the UHPC shell-core concrete interface.The increase in UHPC shell thickness reduces the effective confinement range of the UHPC shell on the core concrete at the joint opening,thereby accelerating the degradation of interfacial bond strength.As the shell thickness increases from 30 mm to 50 mm,the peak load increases by only 4.66%.With the increase of axial compression ratio,the confinement effect of the UHPC shell on the core concrete is enhanced,and both the cracking load and peak load of the specimen increase significantly.The peak load of the specimen increases by 6.62%when the stirrup ratio increases from 0.85%to 1.06%.Furthermore,increasing the stirrup ratio effectively slows down the degradation rate of interfacial bond strength.The specimen with a higher stirrup ratio exhibits the smallest interfacial bond degradation,indicating the best interfacial integrity.Finally,a shear capacity calculation method was proposed based on the strut-and-truss model,showing good agreement between calculated and experimental results.

关键词

梁柱节点/钢筋UHPC模壳/拟静力试验/受剪性能/承载力计算

Key words

beam-column joint/reinforced UHPC shell/quasi-static test/shear performance/calculation of bearing capacity

分类

建筑与水利

引用本文复制引用

王朋,尤学辉,史庆轩,王秋维,戎翀..预制钢筋超高性能混凝土模壳混凝土梁柱节点受剪性能研究[J].建筑结构学报,2026,47(9):14-28,15.

基金项目

国家自然科学基金项目(52578245),陕西省自然科学基础研究实验室重点项目(2025SYS-SYSZD-048). (52578245)