| 注册
首页|期刊导航|重型机械|超高压静液挤压密封结构设计及高熵合金涂层磨损行为研究

超高压静液挤压密封结构设计及高熵合金涂层磨损行为研究

杨建 张雷 张君 罗远新 王勇勤 罗洋 王好

重型机械Issue(5):57-66,10.
✕
重型机械Issue(5):57-66,10.

超高压静液挤压密封结构设计及高熵合金涂层磨损行为研究

Study on seal structure design and wear behavior of high-entropy alloy coating for ultra-high-pressure hydrostatic extrusion

杨建 1张雷 2张君 3罗远新 2王勇勤 4罗洋 4王好4

作者信息

  • 1. 重庆大学 机械与运载工程学院,重庆 400030||中国重型机械研究院股份公司 金属成形技术与重型装备全国重点实验室,陕西 西安 710018
  • 2. 重庆大学 机械与运载工程学院,重庆 400030||重庆大学 国家卓越工程师学院,重庆 401135
  • 3. 中国重型机械研究院股份公司 金属成形技术与重型装备全国重点实验室,陕西 西安 710018
  • 4. 重庆大学 机械与运载工程学院,重庆 400030
  • 折叠

摘要

Abstract

To address the severe wear failure of seals under the 1 500-1 800 MPa working condition of ultra-high-pressure hydrostatic extrusion,a gland-type ultra-high-pressure dynamic seal structure was designed,and a MoNiTaTiV high-entropy alloy(HEA)coating was prepared on GCr15 steel by laser cladding.Taking QBe2.0 beryllium bronze as the counterpart,the high-pressure wear behavior of the coating and the substrate under dry and oil-lubricated conditions was investigated at a contact stress of 1 507.5 MPa.The results show that the designed structure combining an O-ring with triangular metal gaskets achieves low-pressure sealing after pre-assembly,and the triangular gaskets expand laterally to eliminate the clearance as the pressure rises,thus realizing reliable sealing under ultra-high pressure.The coating consists of a BCC solid-solution phase and a TiN ceramic phase,and is metallurgically well bonded to the substrate,with a thickness of about 600 μm and a microhardness of about 1 099.3 HV,which is 3.7 times that of the substrate.The wear volume of QBe2.0 sliding against the coating decreases from 3.73 mm3 and 2.79 mm3 to 0.087 6 mm3 and 0.078 3 mm3 under dry and oil-lubricated conditions,respectively.The friction coefficients of the tribo-pairs are ranked as QBe2.0/GCr15(dry)>QBe2.0/MoNiTaTiV(dry)>QBe2.0/GCr15(oil-lubricated)>QBe2.0/MoNiTaTiV(oil-lubricated),and the average friction coefficient of the coating is reduced by 11.53%and 34.65%compared with the substrate under dry and oil-lubricated conditions,respectively.Under dry sliding,the substrate is dominated by a mixed mechanism of abrasive and adhesive wear,while the coating is dominated by adhesive and abrasive wear.Under oil lubrication,only slight abrasive wear occurs on the coating,whereas abrasive wear,oxidative wear and microcracks appear on the substrate.The results indicate that the MoNiTaTiV HEA coating coupled with QBe2.0 beryllium bronze is a promising anti-wear tribo-pair for seals,providing a basis for the anti-wear design of ultra-high-pressure seal structures.

关键词

超高压静液挤压/密封结构/高熵合金涂层/磨损行为/激光熔覆/铍青铜

Key words

ultra-high-pressure hydrostatic extrusion/seal structure/high-entropy alloy coating/wear behav-ior/laser cladding/beryllium bronze

分类

矿业与冶金

引用本文复制引用

杨建,张雷,张君,罗远新,王勇勤,罗洋,王好..超高压静液挤压密封结构设计及高熵合金涂层磨损行为研究[J].重型机械,2026,(5):57-66,10.

基金项目

金属成形技术与重型装备全国重点实验室开放基金(B2408100,W11) (B2408100,W11)

重型机械

1001-196X

访问量0
|
下载量0
段落导航相关论文