首页|期刊导航|中国铸造|Effect of Mn addition on microstructure and mechanical properties of GX40CrNiSi25-12 austenitic heat resistant steel

Effect of Mn addition on microstructure and mechanical properties of GX40CrNiSi25-12 austenitic heat resistant steelOACSTPCDEI

Effect of Mn addition on microstructure and mechanical properties of GX40CrNiSi25-12 austenitic heat resistant steel

Guan-yu Jiang;Meng-wu Wu;Xiao-guang Yang;Hui Wang;Yu-yuan Zhu

Hubei Key Laboratory of Advanced Technology for Automotive Components,Wuhan University of Technology,Wuhan 430070,ChinaHubei Key Laboratory of Advanced Technology for Automotive Components,Wuhan University of Technology,Wuhan 430070,China||Hubei Longzhong Laboratory,Xiangyang 441000,Hubei,ChinaWescast Industries(China)Co.,Ltd.,Wuhan 430100,ChinaWescast Industries(China)Co.,Ltd.,Wuhan 430100,ChinaWescast Industries(China)Co.,Ltd.,Wuhan 430100,China

金属材料

austenitic heat resistant steelmanganesemicrostructuremechanical properties

austenitic heat resistant steelmanganesemicrostructuremechanical properties

《中国铸造》 2024 (3)

205-212,8

This work was financially supported by the National Natural Science Foundation of China(Grant No.52275370),the Key R&D Program of Hubei Province,China(Grant Nos.2022BAD100 and 2021BAA048),and the Open Fund of Hubei Longzhong Laboratory(Grant No.2022ZZ-04).